Enquiry   |
Downloads   |

POF Shrink Films

Shrink Films
POF Shrink Films
Shrink Films : POF Shrink Films

Polyolefin Shrink Films

  • Polyolefin Shrink Films are now the most sought Shrink Films in the Packaging Industry.
  • These shrink films offer 80% shrinking properties (both directions) along with better transparency and remains odorless when heated and cooled.
  • POF Shrink Films does not emit Chloride on heating, this is an important advantage over PVC Shrink Films.
  • Centerfold POF Shrink Films are used for packaging various products.
  • These films can be used across all industries as these films also comply food grade.
  • Shrink Wrapped products using POF Films can be stored between -60°F till 90°F.
  • POF Shrink Films will have less build up on sealer wires, thereby saving costs on replacement of the sealing wire & routine cleaning.

 

 Brochure   
Get Our Expert Advice :
Captcha
 
 
Technical Details
Gauge Opti 200 : 45
CT-301 30
CT-303 : 42
CT-304 : 55
CT-305 : 70
Minimum Use Temperature Opti 200 : -60°F
CT-301 -60°F
CT-303 : -60°F
CT-304 : -60°F
CT-305 : -60°F
Maximum Storage Temperature (2 year max.) Opti 200 : 90°F
CT-301 90°F
CT-303 : 90°F
CT-304 : 90°F
CT-305 : 90°F
Density
ASTM Test Method : D1505
Opti 200 : 0.93
CT-301 0.9
CT-303 : 0.9
CT-304 : 0.9
CT-305 : 0.9
Impact Strength Peak Load (lbs)
ASTM Test Method : D3763
Opti 200 : 12
CT-301 7.5
CT-303 : 11.4
CT-304 : 14.3
CT-305 : 20
Haze (%)
ASTM Test Method : D1003
Opti 200 : 3
CT-301 3.2
CT-303 : 2.7
CT-304 : 3
CT-305 : 3.9
Gloss (%)
ASTM Test Method : D2457
Opti 200 : 88
CT-301 86
CT-303 : 85
CT-304 : 84
CT-305 : 84
Coefficient of Friction (film-to-film, kinetic)
ASTM Test Method : D1894
Opti 200 : 0.3
CT-301 0.17
CT-303 : 0.19
CT-304 : 0.14
CT-305 : 0.13
Moisture Vapor Transmission Rate (gms/100 sq in/ 24 hrs/atm)
ASTM Test Method : F1249
Opti 200 : 1.6
CT-301 2.2
CT-303 : 1.56
CT-304 : 1.33
CT-305 : 0.95
Oxygen Transmission Rate (cc/ m2/ 24 hrs/ atm)
ASTM Test Method : D3985
Opti 200 : 10200
CT-301 7000
CT-303 : 11970
CT-304 : 9280
CT-305 : 6980
Tensile Strength (x1000 psi)
ASTM Test Method : D882
Opti 200 : 20/20
CT-301 20.9/21.6
CT-303 : 19.1/19.8
CT-304 : 17.7/19.2
CT-305 : 17.4/19.3
Elognation at Break (%)
ASTM Test Method : D882
Opti 200 : 110/110
CT-301 88/105
CT-303 : 92/93
CT-304 : 94/120
CT-305 : 120/130
Modulus (x1000 psi)
ASTM Test Method : D882
Opti 200 : 80/80
CT-301 69/69.6
CT-303 : 65.4/64
CT-304 : 62.3/63.4
CT-305 : 53/63.8
Shrink Tension (psi)
ASTM Test Method : D2838
@ 200°F Opti 200 : 251/503
CT-301 476/664
CT-303 : 313/585
CT-304 : 355/540
CT-305 : 288/573
@ 220°F Opti 200 : 360/579
CT-301 499/641
CT-303 : 420/629
CT-304 : 441/617
CT-305 : 364/623
@ 240°F Opti 200 : 428/650
CT-301 548/578
CT-303 : 537/637
CT-304 : 498/599
CT-305 : 430/596
Free Shrink (psi)
ASTM Test Method : D2732
@ 200°F Opti 200 : 10/14
CT-301 11/17
CT-303 : 10/16
CT-304 : 11/16
CT-305 : 10/18
@ 220°F Opti 200 : 17/25
CT-301 20/30
CT-303 : 18/30
CT-304 : 20/29
CT-305 : 18/30
@ 240°F Opti 200 : 38/47
CT-301 53/57
CT-303 : 53/58
CT-304 : 55/59
CT-305 : 54/58